Wednesday, July 7, 2010

Re: [MW:5884] ASME QW 403.5 interpretation.

Hi Louis,

Yes.You can use this PQR for these three types.Last Sentence of QW 403.5 interpretation is as follows.

If Impact is applicable for that material used in PQR,then you have to do the Impact test additionally as per SEc.IX.


Thanks & Regards,


(Karthik)


Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 7/6/10, james gerald <gerry_tup@yahoo.com> wrote:

From: james gerald <gerry_tup@yahoo.com>
Subject: Re: [MW:5875] ASME QW 403.5 interpretation.
To: materials-welding@googlegroups.com
Date: Tuesday, July 6, 2010, 6:57 PM

Yes Absolutely provided if Impact is applicable then Impact tested at the particular temperature

J.GERALD JAYAKUMAR
00919344954677
 


--- On Tue, 7/6/10, A D <alouis1972@yahoo.co.in> wrote:

From: A D <alouis1972@yahoo.co.in>
Subject: Re: [MW:0] ASME QW 403.5 interpretation.
To: materials-welding@googlegroups.com
Date: Tuesday, July 6, 2010, 11:47 AM

Karthik,
                  Thanks. presently I have one PQR P1 G1 to P1 G2, so can I use this PQR for the below
 
1) P.no 1 G1 to P1 G1
2) P.no 1 G2 to P.no 1 G2
3) P.no 1 G1 to P.no 1 G2
 
The same time I can't catch the last sentence of the QW 403.5
 
The variable does not apply when impact testing of the heat affected zone is not required
by other section.
 
Louis

 


From: Karthik <karthik6684@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Tue, 6 July, 2010 2:46:17 PM
Subject: Re: [MW:5873] ASME QW 403.5 interpretation.

Dear Louis,
Please find below the interpretation of QW 403.5.-Change in Material Grouping.-Supplementary essential variables.
 
QW-403.5 (a)
- When you are doing procedure qualification record (PQR) you have to use the same material type and grade which yo are plan  to use in the production welding.
 
QW-403.5(b)
-  Your actual base metal's P-Number and Group Number to be used in production welding shall match with the P Number and Group Number Listed in QW422 as mentioned in WPS.
 
QW-403.5(c)
- If you want to weld P Number-1Group Number-1 material to  P Number-1Group Number- 1 and 2 material you should have two PQR as follows.
 
01. First PQR shall be P.No.1 Group No.1 with P.No.1 Group No.1
 
02. Additional PQR shall be P.No.1 Group No.1 with P.No.1 Group No.2
 
If you are having the two PQRs as mentioned above ,you can weld same P.Number material with the same group number material as well as different group number.
 

OR

 

If you have the PQR of different P.number and Different Group Number,then you can weld the material with the same P.Number,Group number as well as the combination of Different P.Number and different Group number which you have qualified with the PQR.
 
For example,
 
If you have the PQR of P.No.1,Group No.2 with P.No.3,Group No.1..your Procedure shall be qualified for three types of combination as below.
 
01. P.No.1,Group No.2 with P.No.1,Group No.2
 
02. P.No.1,Group No.2 with P.No.3,Group No.2
 
03. P.No.3,Group No.1 with P.No.3,Group No.1.
 
Thanks & Regards,
 
(Karthik)


Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 7/6/10, A D <alouis1972@yahoo.co.in> wrote:

From: A D <alouis1972@yahoo.co.in>
Subject: [MW:5867] ASME QW 403.5 interpretation.
To: materials-welding@googlegroups.com
Date: Tuesday, July 6, 2010, 9:21 AM

Dear friends,
 
                          Any body can give clear interpretaion detail for ASME sec IX QW 403.5.
 
Louis

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...