Re: [MW:5845] Cracking F-11 material

HI.
REVIEW THE PREHEAT TEMPERATURE Y COOL VERY SLOWLY.
 
AGUSTIN


De: limesh M <limesh78@gmail.com>
Para: Materials & Welding <materials-welding@googlegroups.com>
Enviado: sáb, julio 3, 2010 12:20:06 AM
Asunto: [MW:5834] Cracking F-11 material

Dear All,

While welding of nozzle to nozzle joint (nozzle material F11 - bevels
buttered with Inconel 625) with ERNICr-3, we find cracks.What can be
the probable causes and how we can eliminate it?

Thanks and Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...