Re: [MW:5824] API 1104 Code Interpretation

Dear Limesh,
 

Your interpretation is exactly right.

Actually API 1104 only differentiates between rolling and fixed position and not specifying all groove positions that is 1G, 2G, 5G or 6G.
So the answer to your question is:

"Yes position is an essential variable for welding procedure qualification in API 1104 but it only deals the change of rolling or fixed. Whenever you would move between rolling and fixed position of the pipe, you would have to revise the procedure qualification"

 

 

On Thu, Jul 1, 2010 at 5:15 PM, limesh M <limesh78@gmail.com> wrote:
Dear Friends,
 
Still confusion in my mind.....
 
As per API 1104 clause 5.4.2.4 for welding procedure qualification, a change in position from roll to fixed,or vice versa,constitutes an essential variable.
 
In normal case,
 
Roll welding(1G) - Pipe rolling over rollers and welding carried out by automatic processes like SAW/GMAW.
Fixed (2G,5G,6G) - Normally carried out by SMAW in pipeline industry
 
So I think a change from 1G to other positions or viceversa means an essential variable.
 
I think this clause applicable to a change from 1G to other position(ie, 2G,5G,6G) or viceversa .I think we can use a WPS qualified on any position other than rolled (IG) on all positions except 1G.
 
I really don't know my way of thinking is right or wrong.Expecting some clarification from my seniors and friends in this matter.
 
 
Thanks and Regards,
 
 
Limesh
 
 
 
 
 
 
On Sun, Jun 27, 2010 at 9:19 AM, AGUSTIN JIMENEZ <agumarca@yahoo.com> wrote:
Hi.
 

5.4.2.4 Position

A change in position from roll to fixed, or vice versa, constitutes

an essential variable.

For all position is 6G or 5G+2G.

 

Agustin


 


De: limesh M <limesh78@gmail.com>
Para: Materials & Welding <materials-welding@googlegroups.com>
Enviado: sáb, junio 26, 2010 5:05:53 AM
Asunto: [MW:5750] API 1104 Code Interpretation

Dear All,


Is position an essential variable in API 1104 ? ie, If a PQR qualified
on 5G position as per API 1104 qualifies welding on ALL position or
not?

Thanks and Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...