Dear Dhaman,
 
What was the consumable used for the same joint?.
 
Regards,
Bhavesh Patel
Welding Engg.
ISGEC, DAHEJ,
GUJARAT, INDIA

On Wed, Jul 7, 2010 at 4:57 PM, Dharmesh Mistry <Dharmesh.Mistry@heurtey.in> wrote:

Dear all,

 

Is it required to do PWHT for fillet weld carbon steel (BS EN 10025 S275JR) plate 25mm to the plate (ASTM A387 Gr 11 Cl 2) 18mm THK?

 

Best Regards,

 

Dharmesh Mistry

HEURTEY PETROCHEM

Tel. +91 22 67740074

Cell +91 98207 35814

Dharmesh.Mistry@heurtey.in

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...