Re: [MW:0] Heat input As per API 1104

API 1104 does not require recording or establishing a range for heat input unless the welding procedure is being qualified to Appendix A of the standard.  Heat input limitations are typically client specific and the heat input range can be as large as PQR +/- 20%.  If there are tight toughness and hardness requirements, the tolerance of the heat input range should be less.

Geoff
Pipeline Welding Engineer
Houston, TX



On Mon, Jul 12, 2010 at 2:58 AM, Philip, Taiye (Lagos) <Taiye.Philip@deltaafrik.com> wrote:

Hi Gents,

 

As per API 1104, can the qualified heat input range be established as follows for GMAW process?

 

1. The minimum qualified heat input shall be the minimum heat input recorded during PQR -10%

2. The maximum qualified heat input shall be the maximum heat input recorded during PQR +10%

3. While for SMAW process, Maximum qualified heat input shall be the maximum recorded during PQR.

Pls I want more contribution for clarity of purpose.

 

Regards

Philip Taiye

Principal QA/QC Welding Engineer

(MIPs Quality Control)

DeltaAfrik Engineering Limited

2nd Floor, City Express Bank Building

Plot 1637 Adetokunbo Ademola Street

Victoria Island, Lagos  Nigeria

Phone: +234-1-461-8508, +2341-461-6137 ext. 1257
Cell: +234-(0)-803-803-1396
Fax: +234-1-262-2418

e-mail: taiye.philip@worleyparsons.com

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...