[MW:6109] SSC of carbon steels.

We are reviewing procurement spec for CS Forging ASTM A 694 F51 for
Pipeline (ASME B 31.8/31.4 design spec)
It's sour service NACE MR0175 is applicable.while idenfiying the HIC
and SSC requirements we have some doubts.
Since forging HIC is applicable if Sulphur is more than 0.025% .
while identifying SSC requirements refer to the following section A.2
in NACE MR0175

Carbon and low alloy steels shall comply with A.2.1.2 through A.2.1.9
Carbon and low alloy steels, products and components that comply with
A.2 are, with stated exceptions, qualified
in accordance with this part of NACE MR0175/ISO 15156 without further
SSC testing. Nevertheless, any SSC
testing that forms part of a materials manufacturing specification
shall be carried out successfully and the results
reported.
The majority of steels that comply with the general requirements of A.
2 are not individually listed; however, for
convenience, some examples of such steels are listed in Table A.2,
Table A.3 and Table A.4.

Here my question is our material (A694 F51 )is not identified in the
table (A.2,A.3 & A.4) even though we can comply with sections A.2.1.2
through A.2.1.9 as applicable and consider this material without any
specific SSC testing
Please provide your expertise

thanks in advance
regards,
vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...