Dear Friends
We are qualifying a procedure of SAW process for a particular job as per ASME Sec IX.
The MOC is SS304L.
We are using an imported SAW wire and flux combination: ER308L and compatible flux.
However client wants the SFA number of the SS SAW flux to be mentioned on WPS as we have mentioned SFA 5.9 for ER308L.
Does ASME Sec II part C, 2007 edition mention SFA for SS flux ?
Client is adamant and We are stuckup.
Please advise !
Regards
Prem Nautiyal
PREM S NAUTIYAL
CELL : 9820313278
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
We are qualifying a procedure of SAW process for a particular job as per ASME Sec IX.
The MOC is SS304L.
We are using an imported SAW wire and flux combination: ER308L and compatible flux.
However client wants the SFA number of the SS SAW flux to be mentioned on WPS as we have mentioned SFA 5.9 for ER308L.
Does ASME Sec II part C, 2007 edition mention SFA for SS flux ?
Client is adamant and We are stuckup.
Please advise !
Regards
Prem Nautiyal
PREM S NAUTIYAL
CELL : 9820313278
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments