Saturday, July 10, 2010

[MW:5928] RE: 5927] Copper Base alloys

B171 C61400 is Aluminium Bronz  and C63000 Is also Al bronze but with Nickel.

For welding Al Bronze with Nickel is easier  than other

 

Cost wise no major difference

 

Regards

 

Hegde

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Phirke, Praphulla D (GE Oil & Gas)
Sent: Saturday, July 10, 2010 12:43 PM
To: materials-welding@googlegroups.com
Subject: [MW:5927] Copper Base alloys
Importance: High

 

Dear all,

For one of my project, I have to use Sea water for cooling purpose.

For the same customer has suggested following materials for heat exchanger

 

Shell, Channel, Channel cover & Baffles as ASTM B 171 C61400 or ASTM B 171 C63000

 

I never used such type of materials earlier.

 

Can anyone suggest me which option is best option & why?

Also let me know which is costlier ?

 

Thanks

Praphulla

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...