Dear Members,
 
We had supplied a Finned tube radiator after 1 year in service the header to tube joint getting shearing off near 10-15 mm from weld joint. what will be the reason for the failure.
 
Details are as given below-
 
Tube inside process fluid- Steam at 200 celcius
Tube MOC- SA 240 TP 249
Tube Thickness-2 mm
Header pipe -3"NB sch10s
Header MOC- SA 240 TP 312
Welding Joint- UW 16.1(d)
Welding Technique- GTAW
Working pressure- 15 bar(g).

 

 
PANKAJ
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...