Dear members,
 
What welding sequence should be followed to control the bow type distortion during long seam welding in coke drums?? If any one has established any procedure please let me know:
1. The type of weld edge preparation
2. The diameter of electrode to be used
3. Any stiffners to be welded during setup
 
Regards,
Ankur

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.