DEAR ALL,

Please anybody send to ASME B31.3 hydro test procedure.and as per the
drawing design pressure is 140bar and test pressure is 200bar. i am which
pressure is follow and when i am doing the test the holding time is
4hours.the recorder chart was during the holding time increase the
pressure and temperature.it is correct please tell me.


regards,
anand

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.