Thursday, July 8, 2010

[MW:0] Welding of CS+Alloy825 clad pipies

Dear All
 
We have to weld 20" to 36" pipe spools with following details. Joints cannot be backwelded or cannot do clad restoration from inside.
Material CS+Alloy 825 clad
Thk between 20mm to 54mm
Complete weld with Alloy 625 will be very costly as the thk is high.
What will be the recommended welding consumable combination.
 
Thnaks
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...