Friday, January 1, 2010

[MW:3938] Welder Qlfn. Range wire and strip

Hi gents,
 
I have a query in the Welder qualification. If a welder qualify Overlay in SAW wire; is the welder qualified in SAW strip also?.
Is ASME sec IX obviously explain this range?.
 
Regards,
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements