Nandesh,

 

PWHT requirement is to be cross referred in line with Construction/Design code. In your mail, the applicable design code is missing. However, assuming the design code as B31.3 (2008) for piping, PWHT is mandatory for a thickness >20mm.

 

Regards,
Vasanth


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nandesh Kumar
Sent: 26 January 2010 10:33
To: materials-welding@googlegroups.com
Subject: [MW:4150] ASME SEC IX...PWHT?

 

Dear All,

 

For our LNG piping project, as per ASME SEC IX for a pipe 16 inch OD and Thk 21.44 mm PWHT is manadtory? We are welding root and hot pass TIG and others SMAW.

Material is ASTM A333 .

 

Thaks in advance

Nandesh Kumar A




Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...