I have a requirement to qualify a welder in 2F position for SAW process.

I have referred the test requirement in QW 542.5 of ASME Sec.IX.

For fillet weld qualification, test coupon thickness is given up to 10 mm only.

For SAW Qualification in 2F, shall i use plate thickness higher than 10mm?

Is there any reference/limitations for plate thickness in Sec.IX?

Pl. provide your valuable suggestions.

regards
P.Rao




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...