Dear Mr. Pradeep,
 
Yes you are right. Please throw some more light on this issue
 
Material : ASTM A333 Gr. 6
Design code : ASTM B31.3
Service : LNG line
Impact requirement : yes @ -21° C
 
Thanks for the suggestions.
Nandesh

--- On Wed, 27/1/10, pgoswami <pgoswami@quickclic.net> wrote:

From: pgoswami <pgoswami@quickclic.net>
Subject: [MW:4156] RE: 4151] RE: 4150] ASME SEC IX...PWHT?
To: materials-welding@googlegroups.com
Date: Wednesday, 27 January, 2010, 3:48 AM

Nandesh,

 

Looking at your query, if the material of construction is P No/S No-1 then PWHT is mandatory over ¾" or 20 mm pipe wall thickness. This is the PWHT criteria as per B-31.3 -2008 code.

 

If the design code is not B-31.3 then PWHT requirements of the applicable design code will follow. Do you have impact requirements for LNG piping if so @ what temperature?.

 

If you could provide those details e.g. materials grade, SA 333 Gr1 or 6 , design code, design temperature more comprehensive answers could be provided.

 

Thanks

 

Pradip Goswami, P.Eng

88,Garth Trails Crescent

Hamilton,Ontario, L9B2X1,Canada

Email-pgoswami@sympatico.ca

Email-pgoswami@quickclic.net

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chandra, Vasanthan (Lagos)
Sent: Tuesday, January 26, 2010 5:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:4151] RE: 4150] ASME SEC IX...PWHT?

 

Nandesh,

 

PWHT requirement is to be cross referred in line with Construction/Design code. In your mail, the applicable design code is missing. However, assuming the design code as B31.3 (2008) for piping, PWHT is mandatory for a thickness >20mm.

 

Regards,
Vasanth

From: materials-welding@googlegroups.com [mailto: materials-welding@googlegroups.com ] On Behalf Of Nandesh Kumar
Sent: 26 January 2010 10:33
To: materials-welding@googlegroups.com
Subject: [MW:4150] ASME SEC IX...PWHT?

 

Dear All,

 

For our LNG piping project, as per ASME SEC IX for a pipe 16 inch OD and Thk 21.44 mm PWHT is manadtory? We are welding root and hot pass TIG and others SMAW.

Material is ASTM A333 .

 

Thaks in advance

Nandesh Kumar A

 


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...