RE: [MW:4078] composition manganese less than requirment of ASTM A36

Dear Mr. Tran,

You can go for spectrometer analysis of chemical composition. That is the best method to determine % of elements. PMI test is mainly for identification of materials, it wont show exact values at any point of time. 

Regards

R Vairamuthu




From: vuong.tv@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:4072] composition manganese less than requirment of ASTM A36
Date: Mon, 18 Jan 2010 10:52:58 +0700

Dear All,

 

Please help me in PMI testing for material ASTM A36 thickness over 20.0mm, the composition requirement of manganese is (0.8 – 1.2)%. But result of test is less than 0.8%. Other testings are accepted (tensile, bending, elongation).

 

Please advice me this result is accepted or not.

 

If not, please advice the solution.

 

Thank you in advance.

 

TRAN VAN VUONG



New Windows 7: Simplify what you do everyday. Find the right PC for you.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...