Thank you very much,
Please advice me for detail as blow:
Plate 20mm

Plate 30mm

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pablo Acelajado
Sent: Monday, January 18, 2010 12:09 PM
To: materials-welding@googlegroups.com
Subject: [MW:4073] RE: 4072] composition manganese less than requirment of ASTM A36
January 18, 2010
Hello Tran!
You did not mention the value that you are getting but only indicated that it is lesser than the lower limit. If all other tests are OK, then you need to discuss the matter with your customer for a concession so that it will be accepted.
Thanks.
PJA
SAVE TREES - THINK BEFORE YOU PRINT
From:
Sent: Monday, January 18, 2010 6:53 AM
To:
Subject: [MW:4072] composition manganese less than requirment of ASTM A36
Importance: High
Dear All,
Please help me in PMI testing for material ASTM A36 thickness over 20.0mm, the composition requirement of manganese is (0.8 – 1.2)%. But result of test is less than 0.8%. Other testings are accepted (tensile, bending, elongation).
Please advice me this result is accepted or not.
If not, please advice the solution.
Thank you in advance.
TRAN VAN VUONG