Re: [MW:4139] RE: 4057] CE of SA516 GR.70 with simulation requirement

Since this plate is going to be welded to LAS-SA387 Gr.11 Class 1 plate.So SA516 Gr.70 is going to see same PWHT temp as that for LAS

Regards
Sachin.Sankhe

On Mon, 18 Jan 2010 21:26:35 +0530 wrote
>



The PWHT temperature is very high Instaed it should be 600-620 C





From:
materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On
Behalf Of sachin sankhe
Sent: Saturday, January 16, 2010 1:22 PM
To: materials-welding@googlegroups.com
Subject: [MW:4057] CE of SA516 GR.70 with simulation requirement





Note: Forwarded message attached

-- Original Message --

From: "sachin sankhe"sachin.sankhe@rediffmail.com
To: materials-welding@googlegroups.com
Subject:
















--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...