Thursday, January 21, 2010

[MW:4123] Demagnetization after completion of MPI test

Dear All,

Can any one tell us the various methods / procedure of demagnetizing the weld after completion of Magnetic particle testing on Ferritic steel welds.

Regards,

Raghavendra

Larsen & Toubro Limited
www.larsentoubro.com

This Email may contain confidential or privileged information for the intended recipient (s) If you are not the intended recipient, please do not use or disseminate the information, notify the sender and delete it from your system.

No comments:

[MW:35633] IP Joint