[MW:4082] RE: 4057] CE of SA516 GR.70 with simulation requirement

The PWHT temperature is very high Instaed it should be 600-620 C

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sachin sankhe
Sent: Saturday, January 16, 2010 1:22 PM
To: materials-welding@googlegroups.com
Subject: [MW:4057] CE of SA516 GR.70 with simulation requirement

 

Note: Forwarded message attached

-- Original Message --

From: "sachin sankhe"sachin.sankhe@rediffmail.com
To: materials-welding@googlegroups.com
Subject:

 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...