Sunday, January 31, 2010

[MW:4166] what is SR and how it is done

what is stress relieving in welding, why it is done and can anybody
explain the sr graph, parameters like holding temperature, holding
time,etc. sr is done in same way for preheat and post heat?

thanks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.