Wednesday, January 20, 2010

Re: [MW:4110] Pitting acceptance criteria

Hi,
 
This topic has been discussed several times.
 
Neverthless, there is no spec. for the pitting acceptance.
 
Since the ultimate effect of the pitting is, reduction in thickness, we can apply the thickness tolerence.

If u refer ABS Modu 2008 , they have mention 0.3 mm in thickness reduction, so max. pitting depth is 0.3 mm as per ABS Rules.
 
 

 
On Wed, Jan 20, 2010 at 1:52 AM, Gulam kader <armvasi@gmail.com> wrote:
Dear all,
 
We received one 40" elbow (ASME 16.9) ASTM A 860 material having so much pitting on full external surface. Which standard we can refer for the acceptance criteria? 
 
 
I referred in ASTM A 860, its talks about only depth of surface discontinuity(5% of the nominal thickness),  there is no detail about the area of the pitting allowance.
 
Please help me on this issue. Very urgent
 
Regards,
 
Gulam Kader 

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Thanks & regards,

K.Babu
Welding Engineer, 
Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...