Re: [MW:3930] Filler metal SS316 to ASTM A106 Gr.B

There should be no Problem using E309Mo below 300 degee centigrade, for metal SS316 to ASTM A106 Gr.B.
 
Regards
Chitturi
On Wed, Dec 30, 2009 at 7:28 PM, babu k <kbabupsg@gmail.com> wrote:
Hi gents,
 
On the basis of  metallurgical point of view, is there any effect of choosing E309Mo as the filler metal for the above combination of base metal.
 
Service temp is minus 40 (Max.) 
 
Regards,
 
K.Babu,
Singapore 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...