Re: [MW:3844] Welding of Carbon steel to Duplex Stainless Steel


Hi KC
You can use.
ER309L/E309L-17

Thanks & Regards
----------------------------
Narendra Gohil
Welding Engineer
QAFCO
Ph.00974-4228289(O)
Mo.00974-6044289
Email: ngohil@qafco.com.qa

P Save a tree.  

Please don't print this e-mail unless it's really necessary.



From: KC <kc.chavda07@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: 16/12/2009 08:03
Subject: [MW:3843] Welding of Carbon steel to Duplex Stainless Steel
Sent by: materials-welding@googlegroups.com





Hellow, every body,

for welding of SA 516Gr.70 to SA 182 F51 (UNS 31803) Deuples stainless
steel-2205, which filler wire & Electride we have to use.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...