Re: [MW:3922] WPS & PQR clarification

Dear Friend,
Before doing a new PQR, you have to make a "DRAFT" WPS to run the PQR.
After qualifying the NEW PQR with all the required mechanical tests
and perameter, modify the DRAFT WPS in a correct WPS with supporting
the new PQR with all the correct essential,non essential &
supplimentary essential varialbles(if impact required) as per the PQR.

Regards,

On 12/30/09, mahen dran <cbemahendar@yahoo.com> wrote:
> Dear Group
>
>  Good day,
> --------------------------------------------------------------------------------------------------------------------------------
> Still I have confusion on WPS and PQR terms.
>
> 1. WPS to be created  first , with respect to  selection of process,
> electrode and current  etc.
> 2. PQR is developed  after WPS ,by entering the the actual variation
> relevant to the WPS.
>
> |Corresponding reference numbers are to be entered  in each other.
>
> This is the information  from ASME IX codes.
>  --------------------------------------------------------------------------------------------------------------------------
> But there is a controvercial  statement  from some of our colleques, PQR to
> be developed first and  Supporiting PQR  reference number is to be entered
> in the WPS.
>
> Please clarify this confusion .
>
>
> mahendra
> KSA
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Sukamal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...