Hi freen
In these steel the weldability is good, but most tipes of carbon content can present problems of crack.
Preferably shall by weld with low hodrogen electrode.
Check the carbon content and selecting the filler material.
Kind regards
Gustavo Mendoza
----------- Mensaje Original --------------
De: SLM [smahuri@lntecc.com]
Para: materials-welding@googlegroups.com [materials-welding@googlegroups.com]
Cc:
Asunto: [MW:3840] welding electrode requirement
Fecha: 15/12/2009 04:15:51
Mensaje:
Hi,
Kindly, let me know which welding electrode should be applied for welding of following material
1. IS 1364 to IS 1030 material.
2. Any precautions requirement for welding of above material
The following material is to be used for Gantry Rail
Regards,
Snehkumar L Mahuri
Region Quality Manager
M : 09909914456
"This Message and its contents is intended solely for the addressee and is proprietary.Information in this mail is for L&T Business Usage only. Any Use to other than the addressee is misuse and infringement to Proprietorship of L&T ECC.If you are not the addressee please return the mail to the sender.L&T ECC DIVISION"
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogs pot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments