Tuesday, December 15, 2009

Re: [MW:3837] RT Requirments

Premier Oil specs have 100% RT and PT for all SS instrument air lines.

On Mon, Dec 14, 2009 at 10:46 AM, P. PALANIVEL <p.palanivel@gmail.com> wrote:
Dear Friends Good DAY,
 
Can any one help for the below quiery,
 
A requirement for to replace Pnuematic test in palce of Hydro test for Instrument Air line.  Already there is a requirment of 10% Radiography of the line. What will be the RT required % if Pnumetaic test is carried out.
 
Pl. also let us know where may the requirment is given in CODEs or any other Project spec.
 
 

Thanks & Regards,

 

Palanivel.P

Quality Superintendent.

CAIRN INDIA,

Barmer, Rajasthan - 344 001. India.

Mobile   :   +91 90018 94547 & +91 97904 00797.

E Mail    :    p.palanivel@cairnindia.com

                     www.cairnindia.com

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

Vinod R Upadhyay
SMOE (a subsidiary of SembCorp Marine)
Batam Yard
Mob:+62 815 1474 1550


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...