Dear Friends,Seniors,
Subject:-A312 TP 316L SS, SCH 10S WELDING,DIA 10"
We are facing too many failures with our welders in Welding of SS Sch 10S (Lower Thickness).Even Good welders are not able to give good penetration even with adequate purging.Fusion is not clear.Sometimes the shape changes.
Is it bcoz of the ability of the Welder only or Something extra need to be taken care ?
Anybody can give me useful tips/suggestions to come over this issue? Any useful tips to the welders?
Warm Regards
Ramesh
QA/QC Engineer
Galfar Al Misnad Engg & Contg.W.L.L
Doha-QATAR
THIS IS YOUR DAY..YOU CAN..YES..DO IT...
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subject:-A312 TP 316L SS, SCH 10S WELDING,DIA 10"
We are facing too many failures with our welders in Welding of SS Sch 10S (Lower Thickness).Even Good welders are not able to give good penetration even with adequate purging.Fusion is not clear.Sometimes the shape changes.
Is it bcoz of the ability of the Welder only or Something extra need to be taken care ?
Anybody can give me useful tips/suggestions to come over this issue? Any useful tips to the welders?
Warm Regards
Ramesh
QA/QC Engineer
Galfar Al Misnad Engg & Contg.W.L.L
Doha-QATAR
THIS IS YOUR DAY..YOU CAN..YES..DO IT...
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments