please use appropriate subject line (specify to the query), many times messages are rejected during moderation due to lack of info, and without subject line etc. please take care.
it could be SB209 (not SB290)
ER1100 is suitable, but ER 4043 may be used for some applications. refer SFA 5.10 for selection choice.
you can also check the attachment for selection
you can also check the attachment for selection
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of prashant pansare
Sent: Monday, December 21, 2009 10:13 AM
To: mat wel
Subject: [MW:3858] Filler wire & Electrde Req.
| Dear All, I' ve to weld SB 290 ALUMINIUM 1100, I m using ER 4043,but I m not sure weather it's a pefect filler wire. Is there any chart available to choose appropriate filler wire or electrode for the perticular material? Pl. forward. Thanx in advance & Merry X' mas to all of u. PSP |