Thursday, December 31, 2009

[MW:3933] RE: 3932] Boiler quality steel Vs. Structural quality steel

What type of steel it is? is it specified in UCS 23? , you may use steels like SA36, SA283 Gr A/B/C, provided conditions as specified in UCS6 (b)  are met for Section VIII div 1 vessels


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Agrawal Sunil (Mumbai -Stequ)
Sent: Thursday, December 31, 2009 12:55 PM
To: materials-welding@googlegroups.com
Subject: [MW:3932] Boiler quality steel Vs. Structural quality steel

What is the basic difference between Boiler quality steel and Structural quality steel.

Can we use Structural quality steel if it passes all test of ASME?

 

Best Regards,

Sunil Agrawal


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...