RE: [MW:3850] Reheat cracking in Cr-Mo-V steel welds with SAW welding

Dear Forum Members,

Attached are some information on the reheat cracking of Cr-Mo-V steel welds.
In 2008,this issue was very prevalent. To the best of my knowledge it was
with one specific type of SAW Flux-Wire combinations from certain
manufactures which caused this problem.

Subsequently the following presentations were made in various API forums. I
hope this information would benefit the forum members.API introduced an
appendix on NDE methods for detection of such cracks in RP-934(a draft copy
of this appendix is attached)

There are more information available on the web on reheat cracking, however
they are some company specific, and may not be posted without the presenters
permission.

It would be good to hear from welding consumable manufacturers' on this
cracking issue.

Thanks

Pradip Goswami,P.Eng
88,Garth Trails Crescent
Hamilton,Ontario, L9B2X1,Canada
Email-pgoswami@sympatico.ca
Email-pgoswami@quickclic.net
Tel-905-679-9677

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of PEMMARAJU
RAGHAVENDRA
Sent: Saturday, December 19, 2009 6:42 AM
To: materials-welding@googlegroups.com
Subject: [Norton AntiSpam] [MW:3849] Reheat cracking in Cr-Mo-V steel welds
with SAW welding

Dear All,
Pl.share your knowledge and know-how this new phenomenon of cracking
occurring mainly in highly restrained high thick welds of SAW weld process.
The reasons for this reheat cracking and detection by various NDT methods
can be matter of interest for the forum.


Regards,

Larsen & Toubro Limited
www.larsentoubro.com

This Email may contain confidential or privileged information for the
intended recipient (s) If you are not the intended recipient, please do not
use or disseminate the information, notify the sender and delete it from
your system.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchanged in this group are members personnel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...