Hi KC,
 
Most of them get confused in choosing electrode for this combination,and think to go for Duplex filler wire  / elecrode.
 
But ER 309L is richer filler wire than Duplex ER 2209, hence ER 309 should be used.
 
 
Rgds
K.Sudhakar
Welding Engineer
Singapore
On Wed, Dec 16, 2009 at 1:00 PM, KC <kc.chavda07@gmail.com> wrote:
Hellow, every body,

for welding of SA 516Gr.70 to SA 182 F51 (UNS 31803) Deuples stainless
steel-2205, which filler wire & Electride we have to use.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...