Dear Mahendra,
If you are running WPS for the first time then follow what other friends (
Daniek & Sukamal)suggested. Start with draft WPS , run PQR and finalize
WPS.
If you have many PQR`s in records from previous jobs/project within the
required specs and parameters, then you can issue a WPS based on the
existing one (s) and no need for a fresh PQR.
Regards

Fereidoun


mahen dran
<cbemahendar@yaho
o.com> To
Sent by: materials-welding@googlegroups.com
materials-welding cc
@googlegroups.com
Subject
[MW:3917] WPS & PQR clarification
12/30/2009 04:31
PM


Please respond to
materials-welding
@googlegroups.com


Dear Group

Good day,
--------------------------------------------------------------------------------------------------------------------------------
Still I have confusion on WPS and PQR terms.

1. WPS to be created first , with respect to selection of process,
electrode and current etc.
2. PQR is developed after WPS ,by entering the the actual variation
relevant to the WPS.

|Corresponding reference numbers are to be entered in each other.

This is the information from ASME IX codes.

--------------------------------------------------------------------------------------------------------------------------
But there is a controvercial statement from some of our colleques, PQR to
be developed first and Supporiting PQR reference number is to be entered
in the WPS.

Please clarify this confusion .


mahendra
KSA


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

Save a tree...please don't print this e-mail unless you really need to.


Save a tree...please don't print this e-mail unless you really need to.




This email and any attached files ("Message") may contain confidential and/or privileged information. It is intended solely for the addressee(s). If you receive this Message in error, inform the sender by reply email, delete the Message and destroy any printed copy.
Any unauthorized use, distribution, or copying of this Message or any part thereof is prohibited. Emails are susceptible to alteration. Neither Technip nor any of its affiliates shall be liable for the Message if altered or falsified nor shall they be liable for any damage caused by any virus that might be transmitted with this Message.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...