RE: [MW:3845] welding electrode requirement

AWS D14.1/D14.1M, Specification for Welding of Industrial and Mill Cranes and Other Material Handling Equipment will provide guidance for welding of gantry rails.  It can be purchased from the American Welding Society bookstore at www.aws.org.
 
David Landon
Vermeer Corporation


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of agmendoza@cantv.net
Sent: Tuesday, December 15, 2009 7:36 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:3841] welding electrode requirement

Hi freen

In these steel the weldability is good, but most tipes of carbon content can present problems of crack.

Preferably shall by weld with  low hodrogen electrode.

Check the carbon content and selecting the filler material.

Kind regards

Gustavo Mendoza
----------- Mensaje Original --------------

De: SLM [smahuri@lntecc.com]
Para: materials-welding@googlegroups.com [materials-welding@googlegroups.com]
Cc:
Asunto: [MW:3840] welding electrode requirement
Fecha: 15/12/2009 04:15:51
Mensaje:

Hi,

 

Kindly, let me know which welding electrode should be applied for welding of following material

 

1.       IS 1364 to IS 1030 material.

2.       Any precautions requirement for welding of above material

 

The following material is to be used for Gantry Rail

 

 

 

Regards,

 

Snehkumar L Mahuri

Region Quality Manager

M : 09909914456

 



"This Message and its contents is intended solely for the addressee and is proprietary.Information in this mail is for L&T Business Usage only. Any Use to other than the addressee is misuse and infringement to Proprietorship of L&T ECC.If you are not the addressee please return the mail to the sender.L&T ECC DIVISION"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogs pot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...