Daniel,
 
I attached the interpretation of B-31.3 code on the issue of painting before hydrotest:-
 
  • In ASME, B-31.3-2006 Clause 345.3.1  specifies, All joints, welds (including
    structural attachment welds to pressure-containing components),and bonds shall be left uninsulated and exposed for examination during leak testing, except that joints previously tested in accordance with this Code may be insulated or covered.
 
  • All joints may be primed and painted prior to leak testing unless a sensitive leak
    test is required. The word may is suggestive not mandatory.
 
  • However  the best practice for  painting ,before or after hydrotest may be mutually resolved with client, depending on the interest of the project.
 
  • Painting before hydro test may involve double and redundtant work.Especially if the defect is detected on a painted surface during hydro test.area to be repaired would require the paint to be stripped and repainted after successful repair.
 
 I hope this would  clarify the issue. Appreciate inputs from the others.
 
Thanks.
 

Pradip Goswami,P.Eng

Senior Engineer/Specialist(Welding-Metallurgy)

Component Integrity Dept.

Engineering & Training Services Division

ONTARIO POWER GENERATION Inc.

PO Box-2000, RR-55(South)

Nanticoke, Ontario,N0A1L0

Tel:-(519) 587-2201, Ext 3107--in Nanticoke

         (416) 231-4111, Ext 5925--in Kipling,Toronto

Fax: (519) 587-6814

Email-pradip.goswami@opg.com.


 


Date: Mon, 30 Nov 2009 15:39:12 +0100
Subject: [MW:3771] hydrotest b31.1
From: daniel.iordache@gmail.com
To: materials-welding@googlegroups.com

Hi, 

I have a strange situation about Hydrostatic Test ......

Until now we used to let all welds of piping system no painted........

now our client read in B31.3 and open the discussion that in code is wrote that is allowed to paint the welds before hydrostatic test......

What do you think about that?????

regards

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...