Hi,
 
If you fabriate any reinforcements into two pieces then you need to have the tell tall hole on horizontal axis, in order to find the leaks in horizontal welds,
 
Please refer 3.7.5 of API 650
 
Regards,
 
K. Babu
Singapore


 
On Thu, Jun 25, 2009 at 10:49 PM, navin ullas <navinullas@gmail.com> wrote:
Dear All
As per API 650 the telltale hole for a reinforcement pad should be
kept in horizontal position or axis ,can anybody explain why?
Thank you in advance
--
Navin






--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...