[MW:2574] Re: SA-276 type 316 Bar

Dear Devang,

Welding on 276 Type 410 only pbm It will create crack. A276 Type 316 We didnt faced any pbm. ( We have used this material in Valves.)

On Mon, Jun 29, 2009 at 12:14 PM, Shashank Vagal <nach_sam@yahoo.com> wrote:
Devang,
What welding exactly you want to do here, if you could elaborate on that, the members will be in a better position to answer...
Rgds,
Shashank


--- On Mon, 29/6/09, Devang Patel <devangp@inoxindia.com> wrote:

From: Devang Patel <devangp@inoxindia.com>
Subject: [MW:2570] SA-276 type 316 Bar
To: materials-welding@googlegroups.com
Date: Monday, 29 June, 2009, 11:21 AM


We have a rod of SA-276 TP316 with Condition S, Some of my senior told, welding is not permitted on this rod but i have not found any restriction in ASME code.
 
Can anyone know about it?
 
 
Regards,
 
 
Devang Patel
Manager Engineering
 
INOX INDIA Ltd.
Ph :+91-265-3056392-3056100
Fax :+91-265-2333398-2341449
email :
devangp@inoxindia.com
www.inoxindia.com




Love Cricket? Check out live scores, photos, video highlights and more. Click here





--
Urs . . .
Muthu
Smile make(s)miles ! ! !
Please don't print this e-mail unless you really need to! - this will preserve trees on our planet earth.
Ted Turner  - "Sports is like a war without the killing."
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...