[MW:2556] Re: Does any body knows about water tight weld.

If its not ASME you can carry out vacuum box test, generally its being done for tanks.


From: harish katesia <harish.katesia@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 25 June, 2009 8:15:26 PM
Subject: [MW:2548] Re: Does any body knows about water tight weld.

Dear sir,
 
I am talking for the product of hydro-power plant area, The component has got bowl kind of shape.The size of the component is 6 meter diameter & 4 meter in height.
 
The design has asked to check with 100% U.T. & in addition to this, needs to be check for water tightness.
 
So for such a big size component, filling of water is not feasible, so does ASME codes has any provision to check for water tightness except to fill with water
 
Hydro test also can not be done.

On Thu, Jun 25, 2009 at 3:56 PM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
fill with water, if it doesn't leak its water tight!!
ASME has requirements for hydro test depends on design conditions and the applicable code. 

It is necessary to specify the type of item and applicable code, design conditions etc, to have appropriate answer.


On Thu, Jun 25, 2009 at 2:21 PM, harish katesia <harish.katesia@gmail.com> wrote:

Dear all,
 
Can anybody tell me what is water-tight weld & how to ensure this.
 
Do we have any standards for this or does ASME talks for this.?

--
Regards,
Harish katesia
Mob no.09601551774









--
Regards,
Harish katesia
Mob no.09601551774





ICC World Twenty20 England '09 exclusively on YAHOO! CRICKET
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...