[MW:2552] Re: 2550] D1.1 - WPS - Semi-Auto vs Auto - Need new PQR/WPS

however change +/- 20% oscillation variables needs new PQR, when CVN impact required

On Thu, Jun 25, 2009 at 5:34 PM, Armstrong, Joel <JoelArmstrong@letu.edu> wrote:
Yes, we've done the same thing here with the approval of ABS and no need to requalify.

________________________________

From: materials-welding@googlegroups.com on behalf of ikaria73
Sent: Thu 6/25/2009 8:27 AM
To: Materials & Welding
Subject: [MW:2550] D1.1 - WPS - Semi-Auto vs Auto - Need new PQR/WPS




Hello,
Is a new PQR required if the process is changed from semi-automatic to
automatic?  I am welding piles and would like to use a BUG-O system
with FCAW-GS and already have a PQR/WPS with FCAW-GS semi-automatic.
Can I use the existing PQR to create a new WPS as long as I stay
within the procedures?

Regards








--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...