[MW:2533] RES: 2530] Re: copper

It is a structural repair! All the structure is in copper, is a very old statue.
 
thanks
monica


De: materials-welding@googlegroups.com em nome de T. Paul Coley
Enviada: qua 24/6/2009 11:17
Para: materials-welding@googlegroups.com
Assunto: [MW:2530] Re: copper



Depends on what the repairs are ... is it a structural repair or cosmetic? What material is the main structure? Is this copper sheeting, or overlay, which is thinner. We'll need more data

T.

--- On Wed, 6/24/09, monica <raphaelriccio@gmail.com> wrote:

From: monica <raphaelriccio@gmail.com>
Subject: [MW:2529] copper
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, June 24, 2009, 10:11 AM


Hi,

I have a big copper statue (monument) that i need to repair. which is
the best welding?

thanks,
monica





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...