If the pipe is procured as per  materials pecification and  duly hydro tested at mills and  pipe line segments are tested individually at works , then field NDE would suffice and  end user  may waive off field hydro test. exception to this is any PWHT for field welds done , in such cases exception to Hydro test/ Pneumatric test is not recommended.
Pneumatic test can be done in lieu of  Hydro test subjected to proper precautions, tieing in at various locations are done for safety reasons  based on energy calculations.
Tagore

On Thu, Jun 19, 2008 at 10:53 PM, Rituraj Bose <boser2006@gmail.com> wrote:

Dear Mr. Subramanium,

Please note that RT or any NDT cannot replace Hydro or Pneumatic test.
It can only certify the welded joint, not the whole pipe line.

R. Bose

On Jun 16, 10:21 am, "shiva.subramanium" <shiva.subraman...@wsiko.com>
wrote:
> Dear Members, Mr. Surya and Mr. Raghuram
>
> Due to water problem, you cannot go for pneumatic test based on TP = 110% of
> DP) because the hazard of energy release.
>
> Just calculate the pneumatic pressure for the system
>
> Hydrotest = 60 KG/cm2, so design pressure is around 40 Kg/cm2
>
> For pneumatic test, pressure shall be around 44 kg/cm2.
>
> Imagine the hazard of energy release with reference to the
> attachment(attached previous message of Criticality of Hydrotest pressure vs
> pneumatic pressure)
>
> So, better you can go for 100% RT/UT for all Butt joints and PT/MPT for
> attachment weld as per B31.3 para 345.9.
>
> S. Siva Subramanian
> World Services Italia S.p.A., Kuwait Operations,
> P.O. Box : 28928 - Safat : 13151 - Kuwait.
> Tel : +965 3262945 / 3260338 / 3263987 / 3263691/92, Ext.\ 207
> Mobile - 00965 632 7395
> E-mail :  shiva.subraman...@wsiko.com
>
>
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
>
> [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram
> (Mumbai - PIPING)
> Sent: Monday, June 16, 2008 10:44 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:867] pressure testing
>
> Assuming your design code is B31.3, refer para 345 for the creteria (TP
> is 110% of DP)
>
> Also refer earlier message posted in this group titled  "Criticality of
> Pneumatic pressure test vs Hydrostatic on piping system"
> we should always remember that is necessary to evaluate
> the design aspects of material selection for piping lines to be
> submitted to pneumatic test: in these cases ASME B 31.3 require that the
> materials be guaranteed against their brittleness at the ambient
> temperature during pneumatic test.
> Typical cases are the plants where the ambient temperature could reach
> even minus 50^C (e.g. some parts of Russia).
>
> -----Original Message-----
> From: gajjalla surya prakash [mailto:gajja...@gmail.com]
> Sent: Monday, June 16, 2008 12:32 PM
> To: materials-welding@googlegroups.com
> Subject: pressure testing
>
> dear members,
>
> we are doing hydrotest for the piping systems and now facing the
> problem of water scarcity ,and our customer praposes to perform the
> pneumatic test .
>
> for example hydrotest pressure is 60kg/cm2 what should be the
> pneumatic pressure . where can we get this information.
>
> surya prakash gajjalla.
>
>
>
>  Scanned_ (2).pdf
> 141KDownload- Hide quoted text -
>
> - Show quoted text -




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...