Dear Sachin,
 
Code says about the increase or decrease of time at a temperature. atleast 80 percent of the PQR shall be in production. I am not clear about the time it discuss.
 
2008/6/11 sachin sankhe <sachin.sankhe@rediffmail.com>:

 
Dear Rishi,

Hardness wont be suffucient to accept since we have changed grain structure to certain extent by exceding PWHT temp.resulting in change in mechanical properties.

In that case you need to re-qualify the procedure with new PWHT temperature and all mechanical test to be done as per relevant specification requirement.
If the test passes then we can accept the production joint
If it fails then analysis of failure to be done and results to be conveyed to client.
Based on criticality of the job,let client decide wether to reject or do PHWT gain.
If they propose PWHT again then subsequently we have to qualify procedure with 2 times PWHT.

OTHER MEMBERS ARE ALSO WELCOME TO GIVE THEIR OPINION.

Regards
Sachin.Sankhe


On Wed, 11 Jun 2008 Singh Rishi Raj(Tasnee Site) wrote :


>Dear Friends,
>
>Staying with the subject line of heat treatment, I wanted to know (since
>long ) --------
>
>
>
>What should be done if the temperature while doing PWHT exceeds the
>range mentioned in WPS ??
>
>
>
>For example lets say-
>
>A weld between A335 P11 ( P 4  Gr 1) , thickness 17mm.  WPS ( & B 31.3
>) has the PWHT temp as 704-746 deg C.
>
>If the temp of  PWHT cycle exceeds the higher value by 40deg.
>Centigrade, what should be done?
>
>Can the joint be accepted based on the hardness value?
>
>
>
>Please also provide references with your answer.
>
>
>
>Best Regards,
>
>Rishi Raj Singh
>
>________________________________
>
> From: materials-welding@googlegroups.com
>[mailto:materials-welding@googlegroups.com] On Behalf Of Prabhakar h
>Sent: 09 June 2008 16:25
>To: materials-welding@googlegroups.com
>Subject: [MW:835] Re: Clarification on Heat treatment-Reg.
>
>
>
>Dear Shabbir,
>
>
>
>Thanks a lot for your prompt response and sorry even i cud not catch up
>quite a while as i was held up with my ASME Audits.
>
>
>
>Your Explanation was usefull and it would be better if you cud tell us
>at what conditions we go for the HT and how the same is selected???
>
>
>
>Prabhakar.H
>
>
>
>On 5/4/08, shabbir ahmad <shabbir.ahmad7@gmail.com> wrote:
>
>Dear Prabhakar,
>
>
>
>Nortmalizing: The steel is heated 50 deg. cent grade beyond the upper
>critical tempreture( generally 900 to 940), once the calculated soaking
>time has elapsed the steel is removed from the furnce to cool in still
>air, This produce smaller n fine grain structure that has high toughness
>n strength.In short u can say normalizung makes steel tougher n strong.
>
>
>
>Stress Reliving: Steel heated upto 550-650 d.c..The plastic flow of
>sresses increased as tempr. rises, relieving locked in elastic residual
>welding stress.
>
>
>
>Tempering: The steel is re-heated after hardening and the balance of
>hardness & toughness is adjusted as the temp range 200 - 723deg. cent.
>
>
>
>at 723 d.c. all the martensite has been tempered removing the
>brittleness 7 returning the toughness and some ductility. Normally
>tempering carried out to rebalance the propertied of thermally hardened
>steels.
>
>
>
>solution Annealing : generally carried out on Stainless steel, this
>produces large n coarse grain.Heating the steel above 1040 deg.centi
>grade and quench in oil.
>
>
>
>Thanks
>
>
>
>shabbir
>
>
>
>On 5/3/08, Prabhakar h <hb.prabhakar@gmail.com> wrote:
>
>
>
>      Dear all,
>
>
>
>      Can anyone let me know what is the difference bet'n
>Normallising/Stress releiving/Tempering/Solution anneling..
>
>
>
>      I always get confussed and cudnt get a better idea....
>
>
>
>      Is there anyone to help it out....?
>
>
>
>      Prabhakar.H
>
>      </div
>
>
>>

Sachin.Sankhe
Engineer-Inspection
Aker Kvaerner-Malaysia
Mobile:012-2896901
Email1:Sachin.Sankhe@akerkvaerner.com
Email2:Sachin.sankhe@rediffmail.com


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...
Amity