Skip to main content

[MW:841] RE: 837] Re: STT welding procedure

This is the best example if you are not taking care while posting your query, and time to give more detail and approipriate subject line
STI has been asumed as Friction STIR welding, where you want the details about STT, please take care while posting.

Good Luck!


-----Original Message-----
From: materials-welding@googlegroups.com on behalf of Fly Yalung
Sent: Tue 10/06/2008 10:00
To: materials-welding@googlegroups.com
Subject: [MW:837] Re: Thanx & STT welding procedure

Dear Sir S. N. Dave,
Thank yoy for giving us the information. I have another query this regarding STT welding process, does this effecient to use? Does S. Aramco will require another procedure to be approve? If it will require can you help me to gother information to make a procedure to STT welding process.
Thank you very much for the cooperation.
Best Regards,
Fly L. Yalung - Material Engineer
M. A. Al-Kawari Est.
Ph: 03-5721079
fax: 03-5721471
fly_ma_alkawari@yahoo.com


----- Original Message ----
From: shailesh dave <snd2988@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Sunday, June 8, 2008 6:23:06 AM
Subject: [MW:832] Re: STI Welding


Do you mean STIR WELDING?

REGARDS,

S.N.DAVE

QA/QC MANAGER

TATA PROJECTS LIMITED

IWPP-III, SHAUIABAH, SAUDI ARABIA

fly_ma_alkawari@yahoo.com wrote:

Whom it may concern;
Has anyone had encountered STI welding?

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...