Thursday, May 29, 2008

[MW:814] Re: Clarification requirements for NDT methods

To : Mr Rana

Hi,

ASME V does refer to these methods as acceptable to it. So when you put one the others are taken care of.

And what is CCH70?

Shashank Vagal

--- On Thu, 5/29/08, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
Subject: [MW:812] RE: Clarification requirements for NDT methods
To: materials-welding@googlegroups.com
Date: Thursday, May 29, 2008, 3:40 PM

What is your product? If your product specification refers you must use these standards, of course you can use always Section V in addition to these, but not instead of as these are product specific applications.

 

Like E165 for PT, A275 for MT and A388 for UT, no idea about CCH70


From: Rana Vikas [mailto:vhrana@gmail.com]
Sent: Thursday, May 29, 2008 3:29 PM
To: materials-welding@googlegroups.com
Subject: Clarification requirments for NDT methods

 

Dear All,

 

Hi, I am Vikas Rana working with MNC.

 

I have query during preparation of QAP by selecting method of NDT

 

Can you please clarify differance between below NDT methods

 

ASTM E 165

ASTM A 275 

ASTM A 388

CCH 70

 

Can I put ASME SEC V instead of above methods in QAP ???

If answer no please explain deifferance between them..

 

Early reply most appriable.

 

Regards,

 

Vikas Rana



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...