Tuesday, May 27, 2008

[MW:799] Selection of Gasket/Stud for SS#CS Flanges

Gasket selection mainly depend on Temperature and Pressure of the media, Corrosive nature and Criticality of the application

Since you are using 316 in place of A105, u may use the similar combination of gasket, studs used for a CS#CS joint in the same process stream (since design conditions are same), unless you have contractual requirements if any.


From: Zameer Mohammed [mailto:dreamthinkwork@gmail.com]
Sent: Tuesday, May 27, 2008 10:47 AM
To: materials-welding@googlegroups.com
Subject: SS & CS Flanges

 

Dear Friends,

We have 2 mating flanges, one is SS316 and another is A105. Can I connect SS Flange with CS Flange? In this case, what type of Gaskets, Stud Bolts & Nuts we can use?

For all other CS flanges we are using spiral wound gaskets.

Thank you,

Regards,

 

Sabir


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...