[MW:795] Dissimilar Group number/Thickness combination PQR as per QW403.5/QW403.6

When Impact testing of HAZ is required by design, welding as per ASME SecIX

 

One of PQR qualified with a combination of group number and thickness welded together as 516 Gr60- 6mm thk and 516 Gr 70- 12mm thk

WPS prepared for the range of 6-24mm for both group numbers. (QW403.6)

 

In my opinion it virtually qualifies for nothing (except for 12mm thick) for a combination of group numbers

 

For E.g. I have nozzle SA333 Gr6 and WNRF flange SA350LF2 with thickness of 7.11mm

 

Where as in the above PQR, P#1, Gr#1 qualification range is 6-12mm and P#1, Gr#2 qualification range is 12-24mm and (QW403.5 and 403.6)

 

Please share your views, do my views justified by the correct interpretation of QW403.5 and 403.6?

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...