Mr Sabir,
                          When we are go to diameter above 24" and above, we can't get seamless. Last time my client also looked seamless for 36", but we raised technical query and suggested 100% RT on the weld.
 
So please check with your client.
 
 
Regards
 
Louis

----- Original Message ----
From: Zameer Mohammed <dreamthinkwork@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 12 May, 2008 11:01:10 PM
Subject: [MW:768] Re: A234 WPB & WPBW

Dear Mr. Rushabh,

 

I understand that in SA 234, for WPB there are two method of construction.

Seamless - WPB

Welded - WPBW

 

Is it possible to get Fittings above 16'' as Seamless Construction?

 

I have to procure a 36'' EQUAL TEE and 36'' x 24'' RED TEE. All the vendors are offering Welded Construction, but the Client prefers Seamless. Am I right at the statement that, all fittings above 16'' are Welded Construction only.

 

AM I RIGHT.....?

 

Kindly advice me...

 

Thank you,

 

Regards,

 

 

Sabir



On Fri, May 9, 2008 at 10:53 AM, Nick <rushabh.kapadia@gmail.com> wrote:

Dear Sabir,
Please refer page No.385 of Sec II Part - A (A234).

WPBW is mandatory Marking on the fittings. So the requirements are met
as per A234.

If there is still problem please reply to this.

Rushabh C. Kapadia

On May 8, 1:27 pm, "Zameer Mohammed" <dreamthinkw...@gmail.com> wrote:
> Dear Friends,
>
> As per our specification,
>
> 36'' EQ TEE & 36'' x 24'' RED TEE is C.S. A234 GR WPB BW.
>
> The vendor is offering - C.S. A234 *GR. WPBW*, BW
>
> How can I convince my client that *WPBW *will confirm to the Chemical
> Requirement, Tensile Requirement, for WPB.
>
> Thank you,
>
> Regards,
>
> Sabir





Explore your hobbies and interests. Click here to begin.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...