[MW:765] Re: Joint Factor

 
Actually term is Joint Efficiency
For Full Radiography(100%)-Joint Efficiency is 1%
For spot radiography(85%)-Joint Efficiency is 0.85%

Regards
Sachin

On Thu, 08 May 2008 Zameer Mohammed wrote :
>Dear Friends,
>
>
>
>Whats is Joint Factor in Welded Pipes. We are procuring 24'', 36'' and 42''
>Welded Pipes (EFW). Our client is asking what is the Joint Factor.
>
>
>
>Thank you,
>
>
>
>Regards,
>
>
>
>
>
>Sabir
>
>>

Sachin.Sankhe
Engineer-Inspection
Aker Kvaerner-Malaysia
Mobile:012-2896901
Email1:Sachin.Sankhe@akerkvaerner.com
Email2:Sachin.sankhe@rediffmail.com


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...

JS RED

Pages

Contributors

Blog Archive