You may get Some equivalent grade of NEXTRA 40 or in this catagory
Regards
Hegde P.B.
From: pgoswami <pgoswami@quickclic.net>
To: materials-welding@googlegroups.com
Cc: srinivas.gmsrini@gmail.com
Sent: Friday, 6 May 2011 5:50 AM
Subject: [MW:10957] ASTM 514 equivalent grade material?
From I did in past, it is allowed to substitute material when the following requirement/number of factors are met to the original mat'l (I notice this depends on Client Spec).
1. Carbon content
2. Sulfur composition
3. Phosphor composition
4. Mechanical properties i.e. yield strength, tensile strength, elongation and etc
5. Carbon equivalent (shall not exceed CEQ maximum) or PCM max
6. Impact test (if required by Client)
Have a nice day
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To: materials-welding@googlegroups.com
Cc: srinivas.gmsrini@gmail.com
Sent: Friday, 6 May 2011 5:50 AM
Subject: [MW:10957] ASTM 514 equivalent grade material?
Hello Srinivas,
Attached are the compositions and the mechanical properties of all grades of ASTM A514.The back to back grades adopted for boiler and pressure vessels are classified under SA -517. You may see the comparative descriptions for all the grades concerned.
Since these steels not used for common fabrication work, one has to compare all the properties then only look for substitution. You may not get the exact equivalence and replacement , if so is intended.
If you have any specific issue with this steel feel free to drop a lone.
Thanks.
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Fitria Rahman
Sent: Wednesday, May 04, 2011 10:31 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:10951] ASTM 514 equivalent grade material?
Dear SriniSent: Wednesday, May 04, 2011 10:31 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:10951] ASTM 514 equivalent grade material?
From I did in past, it is allowed to substitute material when the following requirement/number of factors are met to the original mat'l (I notice this depends on Client Spec).
1. Carbon content
2. Sulfur composition
3. Phosphor composition
4. Mechanical properties i.e. yield strength, tensile strength, elongation and etc
5. Carbon equivalent (shall not exceed CEQ maximum) or PCM max
6. Impact test (if required by Client)
Have a nice day
2011/5/4 Srinivas Engr <srinivas.gmsrini@gmail.com>
Dear all.
pl let me know..
wat r equivalent grade material for ASTM 514?
& where we can refer for that?
Is it only chemical composition only..
or any specs tells about this?
Regards
Srinivas
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.